Mould steel selection starts with three questions: how abrasive is the resin, how many parts will the mould produce, and how good must the surface look. A pre-hardened P20 or 718H grade suits large, low-wear parts; H13 or 1.2344 suits high-volume and abrasive work; S136 or 2316 suits medical, PVC and clear parts where corrosion and polish matter. The grade is a system decision, not a label.

What mould steel has to survive: wear, heat and corrosion

Cavity and core steel faces a combination of loads. Every shot wears the gate, the cavity surface and the ejection areas. Hot resin and hot runner systems add heat cycling. Some resins release corrosive by-products, especially PVC and certain flame-retardant grades, and some parts demand a mirror polish that only fine, clean steel can hold.

Heat treatment, mould base rigidity, cooling design and machining accuracy decide how long a mould stays accurate.

P20 and 718H: the workhorses for large, low-wear parts

P20 is a pre-hardened mould steel, typically supplied around 30–34 HRC. It machines well, takes a good polish and is widely used for large parts where wear is moderate: crates, pallets, bins, appliance housings and general industrial components.

718H is a similar family with slightly higher hardness and better polishability, typically around 33–36 HRC. It is a practical choice for large moulds that also need a decent cosmetic surface, and it is easy to maintain and repair locally.

They are not the right answer for abrasive resins, high volume or optical polish, where a harder or stainless grade is usually worth the extra machining cost.

H13 and 1.2344: hot work steel for high volume and abrasive resins

H13 and its European equivalent 1.2344 are hot work steels, usually hardened to roughly 48–52 HRC. They resist wear and heat fatigue better than pre-hardened grades, which is why they are common on high-volume tools and on moulds running abrasive or high-temperature resins.

The trade-off is machining. Harder steel takes longer to cut, drill and polish, and heat treatment adds process steps and lead time. A mould that uses H13 in the cavities and a softer grade in the base is a normal compromise: hard steel where the wear happens, standard steel where it does not.

S136 and 2316: stainless grades for medical, PVC and clear parts

S136 and 2316 are stainless mould steels with good corrosion resistance and excellent polishing behaviour. They are typically used around 48–54 HRC after hardening, and they hold a mirror finish well.

That makes them a sensible choice for medical moulds, PVC parts, clear components and any application where rust stains or polishing defects would be rejected. They are also easier to keep clean between production runs where washdown or humid storage is a factor.

Stainless steel is not automatically the right choice everywhere. It costs more and can be more demanding to machine, so it should be specified where corrosion or polish actually matters. Our medical mould work is a typical example of where the grade choice follows the application.

Matching steel grade to part volume and resin

The quickest way to narrow the choice is to pair volume with resin behaviour:

Application profile Typical steel direction
Large parts, moderate volume, opaque resin P20 or 718H
Cosmetic housings, good polish, moderate volume 718H or a polished pre-hardened grade
High volume, abrasive or filled resin H13 / 1.2344
Medical, PVC, clear or corrosive environment S136 / 2316
High-wear inserts, sliders and cores Hardened insert steel, matched to the local load

Volume is the multiplier. A low-volume tool in a modest grade can be a sensible purchase; a high-volume tool in the same grade may wear out long before the programme ends. The honest calculation includes the cost of a replacement tool.

Hardness, polishing and texture: how steel changes the surface

Hardness affects more than wear. It changes how the steel polishes, how it holds a texture and how it behaves during repair. Softer grades polish quickly but can lose definition on fine textures; harder grades hold detail but take longer to finish.

Texture depth and gloss level should be agreed before the steel is ordered. A texture reference and a gloss target let the mould maker choose a grade and a polishing route that can actually reach the requirement. A finish agreed late becomes a change order.

The resin matters too. Some plastics attack certain steel families, and some release gases that corrode a polished surface between runs. Reading the resin datasheet at the steel selection stage avoids a costly surprise after the first trial. Our plastics material guide explains how the common resins behave.

Where to spend on inserts, sliders and cores

Not every part of a mould needs the same steel. The cavity and core take the wear, but sliders, lifters, wear pads and gate inserts can be even more highly loaded locally. Spending on hardened inserts in those positions often extends tool life more than upgrading the whole base.

The same logic applies to repair. A mould with replaceable inserts can be maintained and, where necessary, updated without re-cutting the entire cavity block. That is a design decision made at the steel selection stage, not a workshop fix later.

Steel verification: certificates, hardness reports and traceability

Steel selection is only real if the grade actually used matches the grade quoted. Ask for the mill certificate, the hardness report and the heat treatment record, and compare them with the quotation and the mould drawing.

Incoming inspection should include hardness checks and a record of the heat number where available. These records matter later, when a mould is repaired, duplicated or relocated. A supplier who cannot produce them is asking the buyer to trust an unverified claim.

SinoMould works under ISO-certified quality management and keeps documented inspection through machining, assembly and trial. The mould quality control process shows how material and dimensional records are handled, and the technical highlights page covers the equipment and inspection side.

Frequently asked questions

Which steel is best for a high-volume injection mould?

For high volume and abrasive resins, a hardened hot work steel such as H13 or 1.2344 is the usual starting point because it resists wear and heat better than a pre-hardened grade. The final choice also depends on the resin, the part geometry, the surface requirement and the mould base design.

Is S136 worth it for medical or clear parts?

S136 and 2316 are stainless grades, so they resist corrosion and take a very high polish. That makes them a reasonable choice for medical parts, PVC and clear components where rust marks or polishing defects would be visible. For ordinary opaque parts in low-wear resins, a well-made pre-hardened grade is often sufficient.

Can I mix steel grades in one mould?

Yes, and it is common. Cavity and core inserts, sliders, lifters and wear pads can use different grades depending on the local load, wear and corrosion risk. Mixing grades is a design decision, so record the reason on the drawing and check it at incoming inspection.

How do I verify the steel grade actually used?

Ask for the mill certificate, a hardness report and the heat treatment record, then compare them with the grade named in the quotation. Dimensional and hardness checks at incoming inspection catch substitution early. A supplier who cannot produce these records is asking you to take the grade on trust.

Does steel choice change the mould price much?

It can change both the material cost and the machining cost, because harder grades take longer to cut, drill and polish. Steel is only one line in the quotation, so compare the whole specification rather than the steel price alone.

Ask our tooling engineers

Send your part drawing, resin and annual volume to [export@sinomould.com](mailto:export@sinomould.com), or contact SinoMould. A tooling engineer will propose a steel grade for each area of the mould and explain the reason, then quote the tool against that specification. SinoMould selects and verifies steel as part of a documented tooling process, not as an isolated line item.

Hardness ranges in this guide are typical values for comparison. Actual steel selection depends on the part, resin, volume and mould design agreed for your project.

Related mould guides

Continue with the next step of the mould project: